SCA-601 Additive for Zinc Plating

SCA-601 Additive for Zinc Plating

Metal Suitability

Iron, Steel, Copper, Nickel etc

Optimum Operating Condition

Temp.: 10 ~ 65 ºC

Conc.: 15 ~ 18 ml/l

Cathode current density: 1 ~ 8 A/dm²

Characteristics

* Potassium chloride base acid zinc plating additive. * Exhibit excellent throwing power. * Suitable for use on both rack and barrel plating.